Tuesday, January 19, 2016

[MW:24139] Re: Qualified thickness for welder

Dear Anamul,

I had checked and agreed with Mr. Padmashankar comments, pls go ahead for discussion with client inspector.

Regards,
Afroz Shaikh
IOTIES

On Tuesday, January 19, 2016 at 7:55:07 AM UTC+5:30, anam...@gmail.com wrote:
Dear Sir,

 We conducted welder qualification at Karbala Oil Refinery Project as per ASME-IX 2013 Edition. 

 WPS details as follow 
1. WPS qualified base metal- P1 to P1 Gruop all
2. WPS mentioned base metal thickness range- 5 to 26 mm
3. Process FCAW
WQT details
1. Joint design Single V butt joint with back weld(Root side back grind then weld)
2. Base metal SA283-C
3. Thickness 16.0 mm
4. Sequence of welding- Root pass>Hot Pass>Filling>Capping>Back grind & Back weld
5. Test position 2G & 3G 

My client inspector say welder will qualified only for 2T  & Pipe Diameter will qualify over 24" I want to clarify is he correct? For thickness qualified he mention about QW-404.30 
However I will appreciate to you for clarify my problem.




Regards
Anamul
QA/QC Engineer


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/93c1b9f9-bbfc-4acf-a838-c303d2b186ef%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...