Monday, January 25, 2016

Re: [MW:24175] welding consumable of S 355 JR

Firstly; you should prepare WPS supporting with PQR and after passing the tessting, you decided to use it. but any way and from our experience you can use E7016 for root in your PQR or use old own WPS and then No problem to use it in production

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...