Follow manufacturer recommendation
--Dear Friends
For how many times you can bake and use the welding Electrodes?
Thanks
Nachhattar Singh
PLEASE THINK BEFORE PRINTING
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Babu Kathalingam
Sent: 20 January, 2016 8:49 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:24146] Expiry period of welding consumables
You can use as long as it is in good condition
On 19 Jan 2016 5:31 pm, <afrozshaikh2007@gmail.com> wrote:
Dear All,
As material test cerificate of welding consumables does not specify validity period for welding consumable, then what is the thumb rule to consider it.
I had checked ESAB Handbook ,it states that max 3 years for electrode if stored as per their guidelines but nowhere i had found information regarding max storage time for filler wire.
Can anyone put light on this topic
Regards,
Afroz Shaikh
IOTIES--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dce3f397-66ba-4993-bd35-86c1c5507cfc%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEAMYiXNad-VtM98AdvjTw5NsSY%2BHO9HQE1p8WLhy050Tmwhmw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001301d15453%24e6f94690%24b4ebd3b0%24%40com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO5%3DVfipYPJN46%3DhJFZNepbO89tSrxfm%3D8dxUof5gjFCQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments