[MW:24137] Re: Thickness Qualification Range of Impact tested WPS for Piping


Dear Biplab,

As QW403.6 & ASME  B 31.3, thickness qualification range will be as mentioned below

Minimum Thickness qualification :(1) If t is more than 6 mm then  min thickness qualifies will be  t or 16 mm whichever is less (2)If t is less than 6 mm then min thickness qualifies will be 1/2 t
 
Max Thickness Qualification: t + 6 mm

Regards,

Afroz Shaikh
IOTIES
On Tuesday, January 12, 2016 at 2:10:35 PM UTC+5:30, Biplab Pal wrote:
Dear Experts,

If impact test is required for any WPS the base metal thickness limit is an supplemental material and qualification of minimum thickness limit shall follow QW-403.6.
Now our Consulting Service Department is telling us the qualification thickness limit shall be t/2 to t+6mm. as per ASME B 31.3 table 323.3.1 for piping.

Guys, did you faced this kind of problem? I am experiencing this problem 1st time.
Please let me know your understanding and experience.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9da8feb1-cca8-4c68-b85e-7d619c164e04%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...