Tuesday, January 19, 2016

Re: [MW:24140] Fwd: mode of metal transfer

It is spray. Ref sec2 partC

On 18-Jan-2016 5:41 pm, "udaya bhaskar" <dusroni@gmail.com> wrote:

Dear experts,

Please clarify which mode of metal transfer we are used  in FCAW 

 Welding Process : FCAW
Gas                      : co2
Filler wire             : AWS A5.20 71T-1C
Mode of metal transfer : ? (Please clarify )


--
With Regards

Udyabahaskar.D

+919676270121

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RN2REbTDX4rvKdo1oUtWMZMz09KaPEPi9TLi70tg5M-BQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN7GsnA1%2BsQHhrmrVb_dVU_4MYKm2RxBSgDyHTaAMdV%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...