Re: [MW:24102] Thickness Qualification Range of Impact tested WPS for Piping

yes construction code (B31.3) limits will apply

On 13 January 2016 at 14:01, 'Biplab Pal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Experts,

If impact test is required for any WPS the base metal thickness limit is an supplemental material and qualification of minimum thickness limit shall follow QW-403.6.
Now our Consulting Service Department is telling us the qualification thickness limit shall be t/2 to t+6mm. as per ASME B 31.3 table 323.3.1 for piping.

Guys, did you faced this kind of problem? I am experiencing this problem 1st time.
Please let me know your understanding and experience.

--
Thanks & Regards
Biplab Pal
Welding Inspector

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3D4cuWpumsK2-NACzY%2BM4Sun-tXbVgVCDXRcDnkta%2Bt_Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...