Did u use extensometer or not?
You have to construct 0.2% offset on the strain axis and get the 0.2% yield strength. Probably ur software would have that option!

2015-10-29 19:13 GMT+04:00 Padmasanker S <padmasanker87@gmail.com>:

Dear all,

Please refer to attached stress -strain graph obtained during tensile testing of SA 106 Gr B pipe.

While performing tensile testing of SA 106 pipes for Div 1 vessels ,we were not getting yield point even though required tensile strength is obtained.

The specimen were taken in both  transverse and longitudinal direction from half thickness.

Kindly share your experience  in finding the root cause..

Please inform if any further details is required for clarity.

Best regards,

Padmasanker,

Quality coordinator,
Bilfal heavy industries ltd.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKDH8Gq%2BubEPKfFeaLTemr8ekcAO-KuOaddmKfrjwLEoDahXYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Mr. Harish.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE4SttGRCQDyJMX957rJZT4Jsu5ZnaT88gLACZwcxz6WLY1dOg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...