Wednesday, October 28, 2015

RE: [MW:23821] PWHT as per ASME B31.3-2014

You should also note that if you are dealing with boiler external piping (BEP), under ASME Section I, the 2014 edition of B31.1 has not been accepted/adopted.  BEP will be designed and fabricated in accordance with the 2009 edition.  The 2009 edition will remain in place until the Section I committee adopts the 2014.

 

Forewarned you are.

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Raghuram Bathula
Sent: Wednesday, October 28, 2015 3:38 AM
To: Materials-Welding
Subject: Re: [MW:23817] PWHT as per ASME B31.3-2014

 

 

 

On 28 October 2015 at 12:27, Himan Nikdin <himan.nikdin@outlook.com> wrote:

Dear Sir

 

Thanks indeed for your quick reply, meanwhile this link"http://www.absa.ca/IBIndex/IB15-008.pdf" does not work any more, would you please send me this PDF file.

 

Regards,

Himan Nikdin

 


Date: Wed, 28 Oct 2015 01:04:38 -0700
From: raghurambathula@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:23815] PWHT as per ASME B31.3-2014

pl. read the link

 

https://groups.google.com/forum/#!searchin/materials-welding/B31.3$2BPWHT/materials-welding/C7TRV2zg3Bk/6OR-EMAiCAAJ

On Wednesday, 28 October 2015 11:51:28 UTC+4, Himan Nikdin wrote:

Dear Experts,

Good Day!!

I have a query regarding PWHT requirements as per ANSI B31.3-2014.

As referred in table 331.1.1 all P.No 1 material shall be subject to PWHT regardless thickness and in table 331.1.3 exemptions to mandatory PWHT mentioned which providing 95ºC preheat applied on material with nominal thickness over 25mm, PWHT can be exempted.

Does it mean "for material with nominal thickness less than 25mm, PWHT is not mandatory"?

 

Appreciated if you share your valuable ideas.

 

Regards,

Himan Nikdin

 

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnHGGhjMM8Vv-9vYgJqNPh4XeQM5LaxR4%2BC5fD6LDNTKg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...