Dear Govin,
please find GAD attached.
Dear Oarag,
please give advise how much air pressure to leak test? our tank capacity is 1400 kL.
Thanks & Regards
On Monday, October 19, 2015 at 12:42:47 PM UTC+8, perumal govindan wrote:
-- please find GAD attached.
Dear Oarag,
please give advise how much air pressure to leak test? our tank capacity is 1400 kL.
Thanks & Regards
On Monday, October 19, 2015 at 12:42:47 PM UTC+8, perumal govindan wrote:
Mr Winarko,
Please share the approved GAD from the Client to clarify further.
Hydro test is proof test, can not be waived off unless Client agrees. Require also calibration of settled liquid on the bottom plate slope.
Regards
GovinOn 13 Oct 2015 16:40, "pras ari" <alhani...@gmail.com> wrote:--WinarkoThanks & RegardsIs any method for substitute leak test? may be NDT or pneumatic test?Dear Sir,Please advise me about leak test (hydro-test) of HSD Fuel Tank, I have 2 (two) tank with capacity 1400 KL, We will held Leak test but but site condition and around very difficult to get water as much as 2800 kilo liters.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com .
To post to this group, send email to material...@googlegroups.com .
Visit this group at http://groups.google.com/group/materials-welding .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .CAMoAFwrSgBgmU-%3DZKEuaK_ YigrM5eBnzrYfTHsyrm% 2BUvMSuYcg%40mail.gmail.com
For more options, visit https://groups.google.com/d/optout .
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eeccc078-d4c9-4421-82df-e31eb131a3c1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments