[MW:23829] Re: composition manganese less than requirment of ASTM A36

Dear Tran,

As for your doubts for carbon steel plates A36,in my opinion,there is no big problem.A36 is just one kind common carbon structural steels.Sometimes,it is replace by steel grade ASTM A283Gr.C(this steel's Mn has no Min.limited,just as Max.0.90%) for many end users.

If you want to know more chemical composition and mechnical property for ASTM A283GrC steel,you also can find on http://www.xinsteel.com/astm-a283-a283m/a283-grade-c.html

So you had better talk with the engineers from your end customer for this point,hope they would accept.Good luck.

Eric from Xinsteel Industrial Co.,Limited

在 2010年1月18日星期一 UTC+8上午11:52:58,Vuongphateco写道:

Dear All,

 

Please help me in PMI testing for material ASTM A36 thickness over 20.0mm, the composition requirement of manganese is (0.8 – 1.2)%. But result of test is less than 0.8%. Other testings are accepted (tensile, bending, elongation).

 

Please advice me this result is accepted or not.

 

If not, please advice the solution.

 

Thank you in advance.

 

TRAN VAN VUONG

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7b5ba752-5d53-4fd9-b94f-1b06f4606a23%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...