Dear Srinivas,

Selection equivalent steel,you should mainly compare their chemical composition and mechnical property.

For checking A36,you can find specification ASTM A36/A36M.

A36 (Yield strength min.250Mpa,tensile strength at 400-550Mpa) is one most common carbon structural steel grade,the equivalent shall be EN 10025-2 S235JR,not S275JR,s275jr steel owned a higher tensile strength and yield strength than ASTM A36.

Else,Jis g3101 SS400 steel,DIN 17100 St37-2,GB /T700 Q235B steel and ASTM A283 Grade C are also similar with ASTM A36 steel.

Regards.

Eric from XINSTEEL INDUSTRIAL CO.,LIMITED

在 2011年1月31日星期一 UTC+8下午9:52:34,Srinivas Engr写道:
Dear All.
pl guide be about in selction of equivalent grade material?
Wat we have to look?
& In which spec we have to refer?
Wat r A36 equivalent materials..?
Wat about S275 grade material?


Thanks & Regards
Srinivas

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/31f188ac-0715-4e75-939d-c800c1a7f6b3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...