Friday, October 30, 2015

[MW:23824] Re: Weld Repair Procedure as per API 1104

Dear Members,

Make defects joints and do the repair work and do the mechanical test and qualify the procedures to satisfy the code and then client requirement,

On Friday, October 23, 2015 at 1:41:34 PM UTC+5:30, waqas suleman wrote:
Dear Members,

We qualified Welding Procedure on API 1104, now our Client is demanding Weld Repair Procedure Qualification.
In scope Weld Repair Procedure Qualification is not mentioned.
I need expert judgement that is it mandatory to qualify Weld Repair Procedure for each welding procedure in API 1104.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/382af72b-0fb2-4f24-a520-78bfda21690e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...