Dear All,

I have situation where Air Receiver Vessel made of SS 316  designed as per ASME SEC VIII DIV 1 U stamped shipped to site but not yet installed. The vessel is stored on warehouse in packed condition.

 

The Present design temperature is 70°C which need to be changed to 85°C.

 

Can you please suggest which are steps we have to take ? Any code reference for recertification ?


 

Regards

Praphulla

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...