[MW:23763] RE: 23760] PTC(Production Test Coupon) Requirements.

Hi Mr Pinaki Boxi.

 

Production test coupons are mandatory as per ASME Sec- VII DIV-2. Please see the generic comparison of the ASME Sec –VIII codes in the following attachment (downloadable at the following web link).

 

The simulation test gives confidence about the materials , not after fabrication. Hence vessel test coupons are required.

 

Please look through following DIV-2 clauses with respect Test coupon requirements (with bullets as below).

 

Thanks..

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist

Hamilton, Ontario, Canada

pgoswami@quickclic.net

pradip.goswami@gmail.com

ca.linkedin.com/pub/pradip-goswami/5/985/299

 

 

http://www.impactrm.com/glossary/ref/ASME_Section_VIII_Comparison.pdf

 

 

 

  • 3.10 MATERIAL TEST REQUIREMENTS
  • 3.10.1 GENERAL
  • 3.10.2 REQUIREMENTS FOR SAMPLE TEST COUPONS
  • 3.10.3 EXEMPTIONS FROM REQUIREMENT OF SAMPLE TEST COUPONS
  • 3.10.3.1 Standard Pressure Parts..
  • 3.10.4 PROCEDURE FOR OBTAINING TEST SPECIMENS AND COUPONS
  • 3.10.4.1 Plates.

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pinaki Boxi
Sent: Tuesday, October 20, 2015 10:10 AM
To: Materials & Welding; Biplab Pal; chandan.majumdar
Subject: [MW:23760] PTC(Production Test Coupon) Requirements.

 

Dear Sir/Experts,

We are going to the manufacturing the Sphere for Liquid/unsaturated LPG.Design Code ASME Section -Vlll Div-2, design temperature -34 deg centigrade. Materials are impacted tested at  -34 deg centigrade wıth simulated heat treatment. Condition.

I have doubt regarding PTC. As per Section Vlll Div-1 if materials are under impact tested in that case PTC is mandatory. 

But as per ASME Section Vlll Div-2 it is required or not please advised me with supporting clause/documents.



--

Thanks & Regards
Pinaki Boxi.
*Manager QA/QC*
*ARP Project Site, Turkey*
*Mob :- +905351054384.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOt02TCwCpbYde3uSevpac%3D8m-HSVO4MdP62%3DQ8D7nvHp6Tnhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...