Experts,

Does the Code allows the Volumetric NDE for Welder Qualification for Unassigned material or similar composition?

I am aware about the exemption which Code states for some P number material and the Code case, but not sure about the Unassigned material/similar composition.

Looking forward for your as usual support.

Regards
Vino, Doha

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7DpkhTHqG2jzggmWFF0cA55t0NX_F1cRLBnCrF6FB0hYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...