Thursday, September 10, 2015

[MW:23442] Re: API 2b straightness interpretation

Dear Vikas,

  Hope you have got the clarification. Please share with me i also have the same doubt. rajutheruvath@gmail.com

On Sunday, 28 July 2013 08:40:01 UTC+4, vikas waghmare wrote:
Dear All,
 
As per the below clause of API 2B

6.4 STRAIGHTNESS

The maximum allowable straightness deviation in any 10-

ft length shall be

1/8 in. For lengths over 10 ft, the maximum

deviation of the entire length may be computed by the following

formula, not to exceed

3/8 in. in any 40-ft length.

My question is , if we have 40 ft length then we have to consider both the point i.e is any 10 ft it shall be max. 1/8" and total length 3/8" or only the second part.

 

Please advise

 

Regards,

 

Vikas waghmare

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/25033e5f-1647-41e0-a9d8-0518783b8a12%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...