Thursday, September 10, 2015

Re: [MW:23440] backchip

You need to revise the WPS but without Re qualification

Sent from my BlackBerry 10 smartphone.
From: Jay Poojary
Sent: Πέμπτη, 10 Σεπτεμβρίου 2015 - 16:51
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:23437] backchip

Dear George Sir,

We welded root & hot pass with GTAW. Did not considered backchip, since it is welded with GTAW. But in production joint we are making this changes. Doing backchip with power grinder.  Does it require requalification.



Thank you,
Jay Poojary.

cordially,
Jay Poojary

On 10 September 2015 at 18:29, <george.dilintas@gr.bureauveritas.com> wrote:

Check QW 410.5 - Method of cleaning
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF71608278.4B3F5AA6-ONC2257EBC.00474509-C2257EBC.004758C0%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DyTURWTdRFSDp0-gVBB5ffzY%3Dio_V6ehTQZRQh7AEeKstA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...