Wednesday, September 9, 2015

[MW:23425] Using ASME IX WPS for replace with AWS D1.1 structure job

Dear all,

I have a situation here. We got steel structure job but my AWS D1.1 WPS not covered for this job. It is possible to replace the WPS WITH ASME IX WPS?. My boss told me to sent the STQ request for replace the AWS D1.1 to ASME IX. I don't have any idea for this. Please guide me. Thank you.

Mohd Firdaus Abd Rahim
QA/QC
+60122796361

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CEC1A20B-5BC3-4448-A2D6-60067EA848D2%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...