The reply below is incorrect: CTOD is not related to cyclic stresses. Both Charpy and CTOD measure fracture toughness. However Charpy is empirical whereas CTOD is a method of measuring material toughness such that the results can be used in fracture mechanics calculations to determine the criticality of material flaws of a known size in that material and corresponding microstructure. CTOD has its notch sharpened by fatigue cracking, but that is to give a very start initiator for the test only. The specimen should be the full thickness of the component to which the test relates, and the test temperature should be the minimum design temperature.

 

CTOD testing is inherently more complex and is much more expensive that Charpy testing and requires laboratories which are rather more specialised than those which can perform Charpy.

 

Alan Denney

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of meisam shokri arfaei
Sent: 23 April 2015 16:36
To: materials-welding@googlegroups.com
Subject: Re: [MW:23150] CTOD AND CHARPY TEST

 

Charpy test is type of test to measure the resistance of a material to shock type stresses whether in room or minus temperatures. 

 

CTOD (Crack Tip Opening Displacement) is for measuring the resistance of material to cyclic type of stresses whether in room or minus temperatures.

 

So the main difference is the type of load which used during the test. So the specimens preparation and test procedures are different.

 

Regards

 

On Thu, Apr 23, 2015 at 12:42 PM, S.Mohammed <mohd52100@gmail.com> wrote:

DEAR ALL

WHAT IS DIFF BETWEN CHARPY TEST AND CTOD TESTING?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9c17d172-8437-41a1-a1bd-4cfe563a9350%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



 

--

M. Shokri Arfaei

ISA-ISTS - Metallurgy Lab. Manager

ASNT NDT Level III

International Welding Engineer

 

Tel.: +98 21 66282127

Fax: +98 21 66282779

Mob.:+98 912 1394023

 

 

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMttz3jzBv4t0Sjna%3DOZUv-M9bnza1ZRa4dcDqYToh-N-oA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...