Charpy test is type of test to measure the resistance of a material to shock type stresses whether in room or minus temperatures. 

CTOD (Crack Tip Opening Displacement) is for measuring the resistance of material to cyclic type of stresses whether in room or minus temperatures.

So the main difference is the type of load which used during the test. So the specimens preparation and test procedures are different.

Regards

On Thu, Apr 23, 2015 at 12:42 PM, S.Mohammed <mohd52100@gmail.com> wrote:
DEAR ALL

WHAT IS DIFF BETWEN CHARPY TEST AND CTOD TESTING?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9c17d172-8437-41a1-a1bd-4cfe563a9350%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMttz3jzBv4t0Sjna%3DOZUv-M9bnza1ZRa4dcDqYToh-N-oA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...