Wednesday, April 22, 2015

Re: [MW:23144] J groove bevel end requirement

Yes I agree with all of you. To reduce heat input,  weld metal and avoid distortion,  J or U groove is preferred.

But, our vendor does not have the facility to do U or J groove.
So, is it acceptable to use V groove above 30mm wall thickness as per international codes.

Thanks & Regards,
G.Prabhakar Raju

On 22 Apr 2015 16:53, "'c sridhar' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
To reduce the weld volume, to control weld cost factor and  to avoid distortion,
we follow certain design norms like:

a. Single 'V' groove say up to 12 to 14 mm,
b. single 'U' groove for 16 to 20 mm
c. Double 'V' groove beyond  20/25 mm
d. Double 'U groove for 30/40 mm
e. single 'J' groove for 50/75 mm and
f. Double 'J' groove for 75 mm and above.

Similarly, Sq. butt without root gap up to 3 mm thick sheet,
Sq. butt with root gap from 4 to 6 and 'V' groove from 6 to 12 mm and like wise.
But there will be overlap in the material thickness selection in above.

But again, there are many constraints like approach to the joint, position of welding,
process selection, plate to pipe joint, quality requirements, availability of machining
facilities  etc. which may change above norms. 

Joint design  is not a mandatory requirement as per codes.But, joint design helps us
to control distortion, which varies from 3 to 9 deg. and said to be max. in single 'V' joint
and less in 'J ' groove type.

Double 'V', 'U' & 'J' helps to keep the distortion down to 2 to 3 deg. But again it depends
up on process selected and size of electrode used (SMAW) etc.

You can check any design manual for joint details.

C Sridhar.
Technical Adviser - Welding,
for Alsta Pristine Engineering, Bangalore

( SS, AL fabricators & A venture of Advance Institute of Welding Technology, Chennai.,
Mobile nos: 0 94449 71097, 0 7406 326326.

Please don't print this e-mail unless you really need to. Save the environment.




 


From: 'raouf salhi' via Materials & Welding <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Wednesday, 22 April 2015 2:00 PM
Subject: Re: [MW:23142] J groove bevel end requirement

dear probhakar ;

It's not mandatory you can always use V bevel but in order to minimise volume of weld metal deposit ,and therefore the welding time, we prefer to use J bevel for thikness above 19 mm.

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258



Le Mercredi 22 avril 2015 4h55, Prabhakar Raj <prabhakarmet@gmail.com> a écrit :


Can anyone give me code reference for J groove bevel end  requirement above 22mm wall thickness.  Is it mandatory to go for J groove.?
---------------------------------------------

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/790943679.1390822.1429700156937.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B-71w-QXwATtVpGbYkG6%2BcknT6MonMGSJw%3D5%3Dg8%3DWN-hgFD7g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...