Re: [MW:23142] J groove bevel end requirement

dear probhakar ;

It's not mandatory you can always use V bevel but in order to minimise volume of weld metal deposit ,and therefore the welding time, we prefer to use J bevel for thikness above 19 mm.

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258



Le Mercredi 22 avril 2015 4h55, Prabhakar Raj <prabhakarmet@gmail.com> a écrit :


Can anyone give me code reference for J groove bevel end  requirement above 22mm wall thickness.  Is it mandatory to go for J groove.?
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B-71w9oYr_5Wb2e8MxKXSn_oWGa2YDv%2BQkOheTDE-D_ZoYRgA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...