Materials Grade -  Base Metal - P1 Gr. 1,2

Type of Weld - One side Bevel Groove and double fillet weld  

Thickness of Separator Shell Plate - 75 mm


Thank you and regards,

Williams

Mobile No. 00968-96004969



On Tue, Apr 21, 2015 at 3:43 PM, Jim Price <JimPrice@polarcorp.com> wrote:

Can you give more specifics on material and grade?

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of williams p wilson
Sent: Tuesday, April 21, 2015 3:32 AM
To: materials-welding@googlegroups.com
Subject: [MW:23135] 2160 PSI - Reparing Separator 2" Nozzles

 

Dear Experts,

 

Greetings..

 

Kindly advice which type of welding procedure & heat treatment for 2", Sch 160  nozzle pipe end joining with 75 mm thick carbon steel body Separator. 

 

Please reply with Pre heating temperature, Intervals of Heating, PWHT Procedures, Welding Rods Details

 

 

Thanks in Advance..

 

Williams.


 

Pictures attached for your reference.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7fysvWYxFHv9cp%3DL%2B-gneiAU0TXosY031wXTaEjuErNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4982f793862d41949aaf0c35302aaa46%40POLARMAIL.PolarTank.local.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ6qoGMOtm-oDNYdO%3DKrGtgHHC3oCmySpeMfRfbK6nyz6Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...