Friday, April 17, 2015

Re: [MW:23121] Change of Brand for SAW Consumables

No in classicification, only brand name is changed which is not essential for no impact requirements. It can be used

On 17-Apr-2015 11:02 am, <george.dilintas@gr.bureauveritas.com> wrote:

This interpretation is too old.
Please refer to the latest edition of the Code Section IX - QW 404.35

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Gurunathan R ---16/04/2015 17:28:46---Please refer the interpretation below. Status:  Currently Valid

From: Gurunathan R <saneguru@gmail.com>
To: Materials-Welding <materials-welding@googlegroups.com>
Date: 16/04/2015 17:28
Subject: Re: [MW:23116] Change of Brand for SAW Consumables
Sent by: materials-welding@googlegroups.com





Please refer the interpretation below.


Status:  Currently Valid
Other Links:
________________________________________________________________________________   
Interpretation:    IX-83-169
Subject: Section IX, QW-404.9
Date Issued: May 14, 1985
File: BC85-089

Question: For submerged-arc welding, can a fabricator use a different brand of flux than that specified in a wire-flux classification for which he is qualified, without performing a new PQR?

Reply: No.


Best Regards,
Gurunathan.R


On Wed, Apr 15, 2015 at 5:22 PM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CACt3NQMvdpRSdPy5%3DYtKhQPuHW58N8oxHWbeaP6xnSqws%3DC3Sg%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF638A3179.D4435A26-ONC2257E2A.001E5636-C2257E2A.001E6C88%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOh4j3xJpqLnuwCgFyUqUaAMiSsdECDgGBU%3D9eqsG_iQw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...