Wednesday, April 15, 2015

Re: [MW:23110] Change of Brand for SAW Consumables


You can change the wps without a need to qualify. 

 

 

Thanks & Regards

 

Firoz Ahmed R. Makrani, PMP


On Wednesday, 15 April 2015 7:48 PM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:


Dear All,
We have PQR of following details:
 
Process SAW with Filler Wire EM12K (ESAB) with Flux F7A8 (ESAB OK 10.62 Flux)
 
Question:
1.       Can we use Filler Wire EM12K (Bohler) with Flux F7A8 (ESAB OK 10.62 Flux)
2.       Can we use Filler Wire EM12K (Bohler) with Flux F7A8 (Bohler Flux)
 
Kindly advise as per ASME Sec IX…with reference.
 
Thanks in advance
 
 
Ali Mhaskar,
QA/QC Manager
Velath Engineering International FZC; Hamriyah FreeZone Sharjah, UAE; * P.O Box 6268 – Sharjah UAE.
(Phone: 00971-6-526 9269, 526 9185, 526 9119 Ext-212 ÈMobile no.: 00971-55 265 3598 ÊFax no. 00971-6-526 9393  üwww.velath.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4htWh-B5O0xAn_yPAbYpWWRcX6NWmDT5tmmziG3jgPAxQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/622566916.1793000.1429109503026.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...