            Kindly share your experiences (special precautions to be taken) during 'Strength Welding of 


            Aluminium Brass Tube -'SB 111 UNS C68700' (78Cu-20Zn-2Alto  

            Aluminium Bronze Tube sheet -'SB 171 UNS C61400' (90Cu-7Al-3Fe).

           

           Thanks & Regards,

 

            ANANTHARAM J

           +91 9840796568

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFV77WoAW89FMQy_sxU%2BkcWYWNsgdDBBG5A2OUdWNayjokmpPQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...