I have some doubt regarding rounded indication (defects) in weld metal.

How much porosities (Numbers with size) are allowed in 3mm to 6mm material thk. According to ASME –VIII, Div-1 (Appendix 4)…

Because, In Appendix 4, FIG 4-3, lot of porosities are showed. So please Guide me.

 

Also suggest me how to read the standard with respect to Appendix-4.

 

I am waiting for your reply in this regards.

 

Thanks & Regards,

K.KANIKUMAR.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACZz93D6agh%3Ds56KR86JpuhQTC04QsmSt5or%2B1GSJcowmNXBMg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...