Hi Lalu,
Even though the chemical properties of ER NiCrMo3 not fully matching with BM chemistry of Incoloy 825 , this filler alloy is widely used because of its availability.
Please look into the attached PDS of ERNiCrMo-14 (Thermanit 686) which is a matching filler alloy and suitable for higher temperature service conditions.
Hope this helps…
With Regards
Amitabha Bhattacharya
Head-Application Technology
voestalpine Bohler Welding India Pvt. Ltd.
voestalpine Bohler Application Technology Centre
M. +91-98 33998246
www.voestalpine.com/welding
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Lalu r p
Sent: Wednesday, November 19, 2014 8:45 PM
To: materials-welding@googlegroups.com
Subject: [MW:22291] Welding of Inconel 625 & Incoloy 825
Dear Experts,
Can we weld Incoloy 825 with inconel 625 consumables ? Since both are under same P number but the chemical combination is different.
Looking forward your valuable response.
regards,
LALU
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment