Re: [MW:22071] Welder Qualification

Hi, my comments are in Red
 
  • If a welder is qualified with CS, can he weld SS.? ( i answered he cannot as F4 and F5 doesn't allow as per ASME Sec IX), but the interviewer told me it can be welded in GTAW with some kind of Gas i forgot the name of it. but i have gone through all the reference code i dont find any as P number and F number are essential variable. He can according to ASME IX QW-423.1.
  • Welder requires tack welding qualification in ASME Sec IX or AWS D 1.1.? As per ASME Sec IX all the welders need to be qualified. As our company manufactures only Tanks and Vessels not much involved with AWS D 1.1, is there any applicable stuff where specifically welder needs to be qualified for Tank welding if he is not qualified welder.?? There is no mention for tack welding qualification in ASME but AWS D1.1 requires tack welding qualification (Part C, 4.32)
Hope this answers your question.
  • If a welder is qualified with ASME Sec IX, can he weld the jobs with the code based on AWS D 1.1.? I have answered yes it's possible as the requirements need to be followed, i.e., Essential variable, Client approval as per AWS D 1.1 Clause 4.2.2.1. Yes he definitely does as ASME IX is more strict and specific to the requirements compared to AWS D1.1.
 

On Saturday, August 30, 2014 12:04:50 PM UTC+8, rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA wrote:
Dear sir
 Plz refer Following
QW-301.2 Qualification Tests.
 Each manufacturer or contractor shall qualify each welder or welding operator for each welding process to be used in production welding and also refer following Interpretation

Interpretation: IX-77-04

Subject:             Section IX, Tack Welder Qualification

Date Issued:      January 31, 1977

File:                  NA

 

   Question:  May a welder be qualified as a tack welder if his tack welds were a part of another

welder's qualification test coupon or part of another welding procedure qualification test which

met the intent of the Code?

 

   Reply:  The Code requires that all welders, (including tack welders), must be qualified per

Section IX.



On Saturday, August 30, 2014 12:25:36 AM UTC+5:30, George Dilintas wrote:

You will not find in the Code the term "tack welder".
The Code is addressing only tack welds. "Tack Welders" are not addressed by the Code.
If tack welds remain in place, then they have to be performed by qualified welders

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor


    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

Inactive hide details for Kannayeram Gnanapandithan ---29/08/2014 06:05:44---tack welder qualification is not mandatory as per Kannayeram Gnanapandithan ---29/08/2014 06:05:44---tack welder qualification is not mandatory as per ASME Sec 9 THANKS & BEST REGARDS

From: Kannayeram Gnanapandithan <kgpan...@gmail.com>
To: materials-welding <material...@googlegroups.com>
Date: 29/08/2014 06:05
Subject: Re: [MW:21739] Welder Qualification
Sent by: material...@googlegroups.com




tack welder qualification is not mandatory as per ASME Sec 9

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Mon, Aug 25, 2014 at 8:05 PM, Shridev Kurup <shridevk20@gmail.com> wrote:

    Tack.1 ..Removal type no need because that potrion welded by unqualified welder does not going to be included in final weld.

    Tack 2.Non removable type  Qualified welder required as per code.

    So it is important you note what type of tacking is ongoing. Like...Bridge tack or something else. Again manufacturer can say they going to remove these unqualified welder welded tacks during the welding.

    Regards
    Shridev

    On 25 Aug 2014 17:12, "Dhanabal Jalachandran" <dhanabal.jalachandrann@gmail.com> wrote:

      Dear,

      Regarding point 2, as you have said, 

      The tack welding is going to be removed.? so the welder may or may not be qualified.? Kindly suggest.

      Point 2-As per code you need to qualified welder for tack weld also because it depends whether tack become part of welding aur you are going to remove it also material, service conditions of equipment.

      BR
      Dhanabal Jalachandran


      On Mon, Aug 25, 2014 at 12:14 PM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

        Dear,

        Point 1 If a welder is qualified in CS for GTAW process then he is qualified for SS with gas backing Argon because for GTAW process deletion of gas backing is essential variable if you carefully go through CODE and for GTAW filler wire SS and CS
        both falls in F NO 6 AS given in code. So CS qualified welder cam make weld in SS and for P no welder is qualified to weld in P1-P15, P34, P41-P43 etc. As per code.

        Point 2-As per code you need to qualified welder for tack weld also because it depends whether tack become part of welding aur you are going to remove it also material, service conditions of equipment.

        Point the 3-If both codes requiement filled and after client approval welder is qualified.
        Best Regards,
        Mohit Aggarwal.

        On 25-Aug-2014 2:10 PM, "Dhanabal Jalachandran" <dhanabal.jalachandrann@gmail.com> wrote:

          Gent's,

          Kindly need your advice to clear one issue based on Welder Qualification.? These questions were asked to me yesterday in Aramco Interview.
          • If a welder is qualified with CS, can he weld SS.? ( i answered he cannot as F4 and F5 doesn't allow as per ASME Sec IX), but the interviewer told me it can be welded in GTAW with some kind of Gas i forgot the name of it. but i have gone through all the reference code i dont find any as P number and F number are essential variable.
          • Welder requires tack welding qualification in ASME Sec IX or AWS D 1.1.? As per ASME Sec IX all the welders need to be qualified. As our company manufactures only Tanks and Vessels not much involved with AWS D 1.1, is there any applicable stuff where specifically welder needs to be qualified for Tank welding if he is not qualified welder.??
          • If a welder is qualified with ASME Sec IX, can he weld the jobs with the code based on AWS D 1.1.? I have answered yes it's possible as the requirements need to be followed, i.e., Essential variable, Client approval as per AWS D 1.1 Clause 4.2.2.1
           
          Regards
          Dhanabal Jalachandran

          --
          To post to this group, send email to
          materials-welding@googlegroups.com
          To unsubscribe from this group, send email to
          materials-welding+unsubscribe@googlegroups.com
          For more options, visit this group's bolg at
          http://materials-welding.blogspot.com/
          http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
           
          The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
          ---
          You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
          To unsubscribe from this group and stop receiving emails from it, send an email to
          materials-welding+unsubscribe@googlegroups.com.
          For more options, visit
          https://groups.google.com/d/optout.


        --
        To post to this group, send email to
        materials-welding@googlegroups.com
        To unsubscribe from this group, send email to
        materials-welding+unsubscribe@googlegroups.com
        For more options, visit this group's bolg at
        http://materials-welding.blogspot.com/
        http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
         
        The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
        ---
        You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
        To unsubscribe from this group and stop receiving emails from it, send an email to
        materials-welding+unsubscribe@googlegroups.com.
        For more options, visit
        https://groups.google.com/d/optout.




      --
      Regards
      Dhanabal Jalachandran

      --
      To post to this group, send email to
      materials-welding@googlegroups.com
      To unsubscribe from this group, send email to
      materials-welding+unsubscribe@googlegroups.com
      For more options, visit this group's bolg at
      http://materials-welding.blogspot.com/
      http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
       
      The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
      ---
      You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
      To unsubscribe from this group and stop receiving emails from it, send an email to
      materials-welding+unsubscribe@googlegroups.com.
      For more options, visit
      https://groups.google.com/d/optout.


    --
    To post to this group, send email to
    materials-welding@googlegroups.com
    To unsubscribe from this group, send email to
    materials-welding+unsubscribe@googlegroups.com
    For more options, visit this group's bolg at
    <font color="#0000FF" face="serif" size
...

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .