Dear All
 
                  Please explain in table 4.5 34) The omission, but not inclusion, of backing or backgouging.
 
If i have PQR qualification test CJP single V butt joint with ceramic backing.
Question.
                     1.) Can i write WPS range qualify to backing gouging CJP double V or Single V butt joint.?
                     2.) And, if i have PQR qualified with back gouging, Can i write WPS range qualify with ceramic backing or not.?
 
 
Best regard.
Sutthipong.K
QA/QC Welding.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...