Saturday, April 26, 2014

Re: [MW:20686] Ladle(heat )analysis VS Product Analysis

Dear Payam,
If you are looking for the reason of these tolerances, Its because of the reactions which could follow after selecting the sample for ladle analysis, but in heat analysis those reactions are stop.

Regards


On Sat, Apr 26, 2014 at 11:27 AM, 'CHINTUKUMAR GANDHI <cgandhi1975@yahoo.com>' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Mr. Payem,

You will have to refer particular product specification/ applicable code.

Thanks & regards,


C. R. GANDHI


From: C.Muni <cmkfc07@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Friday, April 25, 2014 7:26 PM
Subject: Re: [MW:20679] Ladle(heat )analysis VS Product Analysis

Dear Mr.Payem,
You refer ASTM A703 Latest edition.

Regards,


 Chithiran  Muniyanndi,MBA(ISM),PGDCA,PDQM,
Surveyor/Auditor,
Residential Office:
DNV Business Assurance India P Ltd,
29A,Postal Colony,Vicky Nivas,
Off MTP Road,Backside of KSB Pumps,
Narasimhanaickenpalayam PO,
Coimbatore 641031.
Tamilnadu,South India.
Mobile:99947 65591

Growth is the only evidence of life.


On Fri, Apr 25, 2014 at 10:07 AM, PAYAM MAFAKHER <pmafakher@gmail.com> wrote:
Would you please help me ,What is the Tolerance/Deviation in composition BetweenLadle(heat )analysis VS Product Analysis ?
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...