Re: [MW:20638] Can any one explain which one is high grade 304 or 316 & how ?

Dear PK M,
It depends on the application.
316 is not used for urea service
 where we can use 304 Material.
Moly is available in 316 matrial.
It improves pitting corrosion resistance Duplex steel..
Improve high temperature strength and hardness
in Low alloy steel.

Regards,


Muniyandi Chithiran,MBA(ISM),PGDCA,PDQM,
Surveyor/Auditor,
Residential Office:
DNV Business Assurance India P Ltd,
29A,Postal Colony,Vicky Nivas,
Off MTP Road,Backside of KSB Pumps,
Narasimhanaickenpalayam PO,
Coimbatore 641031.
Tamilnadu,South India.
Mobile:99947 65591

Growth is the only evidence of life.


On Sun, Apr 20, 2014 at 10:14 PM, PK M <pkmqaqc@gmail.com> wrote:
Dear ,

Can any one explain which one is high grade 304 or 316 & how ?

Txs.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...