Hi, Good Day!!!

The major difference is that the 316 has about 2% Mo which increase pitting resistance than 304. attached photo will be helpful.

Regards,
Himan Nikdin


Date: Sun, 20 Apr 2014 19:44:08 +0300
Subject: [MW:20631] Can any one explain which one is high grade 304 or 316 & how ?
From: pkmqaqc@gmail.com
To: materials-welding@googlegroups.com

Dear ,

Can any one explain which one is high grade 304 or 316 & how ?

Txs.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...