[MW:20691] Re: B31.3 Piping Ovality limits

Dear mok
there is no straight mention to ovality as per B31.3 and the only presence to diameter tolerance is the next snapshot (332.2 bending)
and i think it can works


 

OUR BEST REGARDS

AHMAD AND MOHAMAD REDA

01223964394 & 01223932379

SENIOR QA-QC

PETROJET 


On Sunday, 27 April 2014 19:51:49 UTC+2, Mok wrote:
Dear Experts,
What are the ovality limits for piping as per B31.3?
Many thanks

Sent from my ThinkPad S230u

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...