[MW:20674] RE: 20669] Ladle(heat )analysis VS Product Analysis

Hello Payam,
 
Please see the extract from API-RP-577, which provides explanations to your query. Ladle or heat analysis is the composition at the and of the melt. Product analysis is the composition  at the end of finished processing.
 
What matters most  in the MTR is the product analysis.
 
Thanks
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
pradip_goswami@yahoo.ca
 

10.8 MATERIAL TEST REPORTS

Materials test reports, sometimes can be a very valuable tool for the inspector and welding engineer. These are typically notarized statements and are legally binding. There are typically two types of test reports, a heat analysis and a product analysis. A heat analysis, or mill certificate, is a statement of the chemical analysis and weight percent of the chemical elements present in an ingot or a billet. An ingot and a billet are the customary shapes into which a molten metal is cast.

These shapes are the starting points for the manufacture of wrought shapes by the metal-forming process, such as rolling, drawing forging or extrusion. A product analysis is a statement of the chemical analysis of the end product and is supplied by the manufacturer of the material. These reports can be supplied for any form of material, including wrought products, such as plate, pipe, fittings or tubing, castings and weld filler metals. The product analysis is more useful to the inspector and engineer since it provides a more reliable identification of the actual material being used for new fabrication or repair of existing equipment.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PAYAM MAFAKHER
Sent: Friday, April 25, 2014 12:37 AM
To: materials-welding@googlegroups.com
Subject: [MW:20669] Ladle(heat )analysis VS Product Analysis

Would you please help me ,What is the Tolerance/Deviation in composition BetweenLadle(heat )analysis VS Product Analysis ?

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...