Friday, April 25, 2014

[MW:20672] RE: 20669] Ladle(heat )analysis VS Product Analysis

You have to read that from the specification for the material of interest, where the permitted tolerances should be stated.

 

Alan Denney

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PAYAM MAFAKHER
Sent: 25 April 2014 05:37
To: materials-welding@googlegroups.com
Subject: [MW:20669] Ladle(heat )analysis VS Product Analysis

 

Would you please help me ,What is the Tolerance/Deviation in composition BetweenLadle(heat )analysis VS Product Analysis ?

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...