Maybe you are referring to the low carbon versions of 304 and 316 (304L and 316L) which have reduced carbon. With this low carbon comes a reduction in the risk of intergranular corrosion in the weld heat affected zone. With the standard grades this corrosion is caused by the carbon combining with the chromium to form chromium carbide, removing the chromium which would otherwise be available to form chromium oxide on the surface of the stainless steel. Stainless steel is only stainless because of the chromium oxide layer on the surface.

 

Alan Denney

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PK M
Sent: 20 April 2014 18:44
To: materials-welding@googlegroups.com
Subject: [MW:20631] Can any one explain which one is high grade 304 or 316 & how ?

 

Dear ,

 

Can any one explain which one is high grade 304 or 316 & how ?

 

Txs.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...