Sunday, April 20, 2014

[MW:20626] Re: Temperature Measurement in Submerged arc welding

Thanks for reply..if i want to measure the temperature via thermocouple which thermocouple will me best suited? what should be the thermocouple location and tip diameter. can i corelate the microstructure formed and cooling rate?

On Friday, 18 April 2014 23:42:29 UTC+5:30, Arya Harish wrote:
Anyone can provide the idea to get the cooling rate through temperature measurement in submerged arc welding?? i need this for welding research purpose.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...