Tuesday, April 1, 2014

[MW:20454] CRA Material

Dear All master,
 
Our supplier proposed material grade SM 2535 / SM 2035 for CRA OCTG with the following reservoir parameter:
Reservoir Temperature: 305 F
Reservoir Pressure: 8105 Psi
CO2 content 6.59 %
H2S Content : 0.59 %
CO2 Partial Pressure: 534 Psi
H2S Partial Pressure: 47.82 Psi
Can we use the material grade SM 2535 / 2035? Which one is better? Please advice. Thanks in advance..
 
Regards,


Lukman

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...