Dear fiend,
For fully austenitic stainless steel e.g., grade 302 longitudinal speed is about 5700m/s and for transverse mode is about 3120m/s.
In case of duplex you have to find the speed (long. or trans. mode) experimentally because you faced with a duplex microstructure of ferrite (microstructure for simple carbon steel) and austenite (microstructure for some stainless steels such as 302). But from my sight you can not use individual speed for ferritic C.S. or austenitic S.S.
Regards
On Thu, Jan 2, 2014 at 9:01 AM, Kale, Bhaskar M <bmkale@gmail.com> wrote:
YOU CAN CALCULATE ACTUAL VELOCITY IN THE MATERIAL.BHASKAR--On Thu, Jan 2, 2014 at 9:38 AM, <think.differently360@gmail.com> wrote:
Saravanan,
The basic of UT sound of velocity of Steel alsmot same including SS and CS. But to know exactly you have to calib on standard block of which material to be used.
On Tuesday, December 17, 2013 6:56:13 PM UTC+7, saravanan sornam wrote:Thank you Mr.Prem , do you have any material for my reference.
Regards
Saravanan
KoreaOn Dec 17, 2013 1:38 AM, "prem nautiyal" <prem_na...@yahoo.com> wrote:--HiI think You can consider the velocity of sound as steel for this material.For longitudinal waves, take V = 5900 m/secFor shear waves, take V = 3200 m/secRegardsPrem Nautiyal9769316004
On Monday, December 16, 2013 10:00 AM, Saravanan Sornam <sarava...@gmail.com> wrote:To post to this group, send email to material...@googlegroups.com--
Dear Experts ,What is the Ultrasonic Velocity to be used for Duplex UNS 31803 material welding examination.Please share some data and material copy for my reference.Awaiting for your reply.Thanks and Regards,Saravanan,Korea.
To unsubscribe from this group, send email to materials-weld...@googlegroups.comTo unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.comTo unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
धन्यवाद,
भास्कर मनोहर काळे
+60149129098--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer
Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment