Re: [MW:16641] RE: 16625] Current/Voltage Requirement for wire 1.6mm for GTAW welding.

Mr. Pandit,

Unless you indicate details like, 
Material used, its thickness, plate / pipe, position of welding, whether it is a groove butt (or) fillet,
pressure / flow / structural etc., it will be difficult to help.

Sridhar.

From: Dinesh <som.din@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 30 January 2013 12:35 PM
Subject: [MW:16637] RE: 16625] Current/Voltage Requirement for wire 1.6mm for GTAW welding.

Dear sir,
 
You are going to weld on CS or SS, Generally interpass temp is approx 190 c but again based on group of material.
Regarding about welding parameters you can refer an welding supplier cartoon & documents  for setting electrical parameter ,generally vary in root pass ,hot pass & Capping. Also based on the travel speed.
 
Heat input = v*I/ travel speed.
 
Regards
 
Dinesh
Pune @ desk of dubai
 
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Anant Pandit
Sent: Wednesday, January 30, 2013 10:26 AM
To: materials-welding@googlegroups.com
Subject: [MW:16625] Current/Voltage Requirement for wire 1.6mm for GTAW welding.
 
Dear Experts,
 
i want information regarding GTAW welding. I am going to use 1.6mm filler wire, can anybody tell what temp/current/voltage to be maintain..
 
its urgent... please give your valluable reply...
 
Regards,
 
ANANT D PANDIT
For SAFESS QUALITY MGMT PVT. LTD.
PUNE.
MOBILE NO.-: +919604348931
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...