Re: [MW:16578] RE: 16574] ASTM A516 Gr.70 normalizing

And the plate must have a mark of "MT" (denoting material treated) . See SA 20, 13.1.2.

Valeria



De:        "John Henning" <jhenning@deltak.com>
Para:        <materials-welding@googlegroups.com>
Fecha:        23/01/2013 14:29
Asunto:        [MW:16577] RE: 16574] ASTM A516 Gr.70 normalizing
Enviado por:        materials-welding@googlegroups.com




See 5.1 and 5.2 of the A516 specification.
 
Anything less than 1.5 inches thick is usually as rolled and anything above 1.5 inches thick is required to be normalized.
 
If you need low temperature impacts and the material thickness is less than 1.5 inches, you should specify that the material be normalized.
 
Heat treatment should be stated on CMTR.
 
John A. Henning
Welding & Materials
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of M2M
Sent:
Tuesday, January 22, 2013 8:47 PM
To:
materials-welding@googlegroups.com
Subject:
[MW:16574] ASTM A516 Gr.70 normalizing

 
 
Dear All
 
I need to know how can understand that ASTM A516 Gr.70 is normalized or not?
 
Somebody told me:
 "according to clause 5.3 of ASTM A516 standard (attached), when we apply charpy impact test on a material and it pass the impact test successfully, we can say the material is surly normalized but if the material can't pass the impact test, we shall apply metallographic test to understanding if the material is normalized.
 
And somebody said me:
"we have just 1 way to know that is the material normalized or not. And its metallographic test."
 
M. Farhang
 
 
 
 
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

__________________________________________________________________  La información contenida en este mensaje es confidencial, y puede ser usada exclusivamente  por aquellas personas a las cuales está dirigida, dentro de los límites establecidos para   su uso. Si este mail es recibido por error, agradeceremos a su receptor tenga a bien informar   esa circunstancia al emisor, dirigiendo el mensaje a la dirección de correo electrónico que  lo haya remitido. En tal hipótesis, además, se solicita no copie ni revele el mensaje, como   así tampoco divulgue su contenido a terceras partes, para evitar un eventual comportamiento   ilícito. Las opiniones contenidas en este mensaje son exclusivas de su emisor y no representan   necesariamente la opinión de la empresa.    The information contained in this message is confidential, and is intended exclusively for the   individuals who have been specifically addressed, considering the limitations established for   its use. If this mail is received by error, please inform the sender and return the message   to the email address that had sent it. In such case, please do not copy or disclose the   message or its contents to any third party in order to avoid any unlawful conduct. The statements   included in this message belong only to the sender and do not necessarily constitute the   company s view.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...