Re: [MW:16551] P11 alloy steel Grade Material - PWHT scope

to avoid PWHT, u should have done preheat(120deg celsius) while welding.

Pandithan, AWS-CWI,CSWIP3.1
Welding Consultant

On 1/18/13, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
> Thank you Ramon,
>
> Did you have some ASME references !
>
> Regards.
>
> 2013/1/18 ramón ignacio briceño <bricenori@hotmail.com>
>
>> Hi Zakaria, P11 require PWHT when you not reach the limit of hardness
>> recomended by the Codes in the Welding and ZAC. Remember, you are work
>> with
>> a material like low alloy carbon steel (Cr-Mo) that is self quench in
>> air,
>> where the welding adquire high hardnees and residual stress not
>> recomended
>> to put it directly in services that demand critical conditions. Such
>> situation requires apply PWHT.
>> Attention with this material.
>>
>> Regards,
>> Ramón Briceno
>> Metallurgical Specialist.
>> ------------------------------
>> From: raghurambathula@gmail.com
>> Date: Wed, 16 Jan 2013 13:34:38 +0530
>> Subject: Re: [MW:16523] P11 alloy steel Grade Material - PWHT scope
>> To: materials-welding@googlegroups.com
>>
>>
>> Nominal wall thickness is the thickness listed in the product
>> specification and not the measured thickness. in your case 12.7mm is the
>> applicable thickness
>>
>> On Wed, Jan 16, 2013 at 1:22 PM, Zakaria ghrab
>> <zakaria.ghrab@gmail.com>wrote:
>>
>>
>> Dear experts,
>>
>> I have one doubt.
>>
>> We have P11 alloy grade material pipe, size 8" SCH 80, thickness = 12.7
>> mm. So according ASME construction code PWHT is not mandatory.
>>
>> For the same piping, we had one non conformance (pipe damage before
>> installation). To release and close, client request to confirm thickness
>> and dimensional check. We get for thickness measurement around 15 mm for
>> all pipie lenght.
>>
>> So, now client request to perform PWHT for welding joints related.
>>
>> ISO Dwg mention 8" SCH 80.
>>
>> How we can release ?
>>
>>
>> Regards.
>> --
>> *زكرياء غراب
>> **GHRAB Zakaria** *
>> +212606588856
>>
>>
>>
>>
>>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>>
>>
>
>
>
> --
> *زكرياء غراب
> **GHRAB Zakaria** *
> Jorf Lasfar Units 5&6 Power Plant construction Project
> EA2C/ SDEM Entreprises
> Site QA/QC Manager
> Mobile : Morocco (+212) 6 61 07 00 11
> Tunisia (+216) 96 635 805
>
>
> Yesterday is the pass, tomorrow is the future; and today? Today is the
> present, the gift: Enjoy it!
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...