Wednesday, January 30, 2013

[MW:16646] Bolts grade differences

Dear All,

In our project for storage tanks (API 650), contractor has supplied
bolts/nuts of A 307 grade where as spec. calls for A 193/194. Even
both are acceptable by 650, but A 193 being the superior quality, how
this can be affected the general quality especially in the long run of
the tanks?. Kindly share your views.

Thanks in advance
Kumar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.