[MW:16605] Re: Leakage during Silo Pneumatic test at 1 bar

Have you tried replacing the gasket with a thicker, softer rubber. Also, ensure that no foreign material is trapped between the flange and the gasket. 

Regards

Swamy
Retired QA Metallurgist, 
Nuclear Fuel Complex,
Hyderabad



On Thursday, January 24, 2013 5:56:02 PM UTC+5:30, mhaskar aly wrote:
Dear Experts,
 
We are trying to do Pneumatic testing of SS silos (4mmthk shell thk) 3.5m dia x 12.0m Long
 
We are observing leakage at plate flange of bottom Cone .
 
Gasket used is 3mm rubber..
 
Can you suggest on this issue...
 
Silos is foe wheat storage application
 
Water fill test is not being done due to less thickness 3 or 4mm
 
Ali Mhaskar
FREE Animations for your email - by IncrediMail! Click Here!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...