Friday, January 25, 2013

[MW:16591] Re: Standard Reference for Hardness of A 516 Gr.70

Dear All,

In addition to trailing mail.

The Vessel is used for storage of Helium liquid.

The PWHT was done according to UCS-56.

The Thk. of Shell & d/e are 40 & 50mm respectively.

The clients wants to know acceptance reference standard of Hradness.

We checked after PWHT & found in range from 150 to 200 HB.

Please provide reference acceptance standard for the Hardness to convince client.

Awaiting your reply.

Regards,
Vikas Rana


On Mon, Jan 21, 2013 at 10:59 AM, Rana Vikas <vhrana@gmail.com> wrote:
Urgent matter. Please guide.


On Mon, Jan 21, 2013 at 10:06 AM, Rana Vikas <vhrana@gmail.com> wrote:
Dear All,

Please provide acceptance value of Hardness for A 516 Gr.70 after PWHT  with Standard reference.

The Vessel is design ASME SEC VIII. The Vessel will be used for cryogenic liquid storage.


With Regards,
Vikas Rana




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...