Monday, January 21, 2013

[MW:16550] Leak Test/Hydro Test/Visual

Hello!!
Our client line list specifies "Visual" for some UG lines. Does this mean checking the line/joints by filling water to the operating/design pressure or only check the visual condition of the weld joint after welding.

Thanks,
Kiran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 