Saturday, December 22, 2012

Re: [MW:16299] Query about Material Identification


I hope, it is AWS A5.01; not AWS 8501.

As per AWS A5.01 (Filler Metal Procurement Guidelines), there are 'lot classification' which is used for batch testing of consumables as per the said standard viz.,
  • C - Covered Electrodes
  • T -  Tubular Electrodes
  • S -  Solid wires
  • F - Flux for SAW

Class S3 : A Class S3 lot of bare solid electrodes and rods, brazing and braze welding filler metal, and consumable inserts is the quantity of one size produced in one production cycle from one heat.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Fri, 21/12/12, Don Bosco Maritime Academy <donboscomarine@vsnl.net> wrote:

From: Don Bosco Maritime Academy <donboscomarine@vsnl.net>
Subject: [MW:16295] Query about Material Identification
To: materials-welding@googlegroups.com
Date: Friday, 21 December, 2012, 10:51 AM



Dear All,

We would like to know what does the S-3 Classification mean as per AWS 8501?  We believe it is a nickle base alloy but will appreciate if more light can be thrown on this. 

Regards,

G. A. Soman
PRINCIPAL


--

DON BOSCO MARITIME ACADEMY
Premier Automobiles Road, Opp. HDIL Complex,
Kurla West, Mumbai 400070
Tel: 2504 1585 / 2018; 25036344. Fax: 2504 0682
Mobile No:  9819451277
Email donboscomarine@vsnl.net
Website www.dbma.in

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...