Sunday, December 2, 2012

Re: [MW:16103] RE: 16090] PAUT for Vessel in Lethal Service

 
What should be the Name plate stamping detils, if we do PAUT or TOFD in lieu of RT.
Originally RT-1 Vessel, if we happen to do  PAUT for Closing joint, then what sould be the stamping on Name Plate..
 
Regards
Raghava
 
 
 
On Sat, Dec 1, 2012 at 7:09 PM, pgoswami <pgoswami@quickclic.net> wrote:
Hi Purav,
 
PAUT or TOFD are accepted by ASME code in lieu of radiography for new construction..Please seethe attachment which references 3-ASME code cases.You may get these ASME  documents in IHS website.
 
Thanks.
 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Purav Desai
Sent: Friday, November 30, 2012 4:29 AM
To: materials-welding@googlegroups.com
Subject: [MW:16090] PAUT for Vessel in Lethal Service

Dear Member,
 
Is it alllowed to use ultrasonic examination(PAUT) in lieu of Radiography for vessel intented to be used in lethal service?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...