Thursday, October 4, 2012

Re: [MW:15465] During WQT , Visual passed by client but RT failed.

thank you for your information,at the same time let me know,in which area of AWS D1.1 saying like this.
 
Thanks and Regards
Sasikumar.R

On Wed, Oct 3, 2012 at 3:43 PM, Kaushik bhagvandas patel <kaushik21185@gmail.com> wrote:
Dear Sir,

As per AWS D1.1 standard sais that the Client is acccepted the welder qualified as per Pre Visual Inspection but With out RT is not possible to qualified the Welder. but With out RT film Welder is not qualified.

Regard's
Kaushik patel
BVIL

On Wed, Oct 3, 2012 at 6:14 AM, Sasikumar.R <sasikumar@punjlloyd.com> wrote:
Dear all experts
 
Goodmorning to all. Kindly clear my doubt about welder qualification as per AWS D 1.1.During WQT 12 welders visually accepted by client, at the same time 3/12 only passed in the Radiographic Test. Can I argue with client to qualify the welder eventhough they failed in the RT. Because normally a welder visually qualified means he will be able to pass in the RT also. suppose if the welder will qualify by the client, that welders they are going to weld minor structual welding only. Can or Can not ?.Any codes or standards saying about this ?
 please advise me.
 
Thanks and Regards
Sasikumar.R

This e-mail and any files transmitted with it are for the sole use of the intended recipient(s) and may contain confidential and privileged information. If you are not the intended recipient of this communication, we request you to notify the sender immediately by return email and destroy all copies and the original message. Any unauthorized review, use, disclosure, dissemination, forwarding, printing or copying of this email is strictly prohibited.
The recipient acknowledges that Punj Lloyd Limited or its subsidiaries and associated companies (collectively "Punj Lloyd Group") are unable to exercise control or ensure or guarantee the integrity of/over the contents of the information contained in e-mail transmissions and further acknowledges that any view, opinion or advice expressed in this message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Punj Lloyd  Group.
Although we have taken all reasonable precautions to ensure that this communication is free from viruses. We do not assume responsibility for any loss or damage arising from the use of this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Thanks & Regard's


Kaushik Patel,
Surveyor,
Bureau Veritas - Gandhidham
63, Shivdhara Nagar,
Plot No. 163, Nr. Purshottam nagar,
Adipur - Gandhidham.
Mobile: +91 9687000073, 9427599638.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
SASIKUMAR.R,
WELDING ENGINEER,
PUNJLLOYD LIMITED,
FTP PROJECT,
BANGKOK-THAILAND.
GSM  : +66832209809.
 


This e-mail and any files transmitted with it are for the sole use of the intended recipient(s) and may contain confidential and privileged information. If you are not the intended recipient of this communication, we request you to notify the sender immediately by return email and destroy all copies and the original message. Any unauthorized review, use, disclosure, dissemination, forwarding, printing or copying of this email is strictly prohibited.
The recipient acknowledges that Punj Lloyd Limited or its subsidiaries and associated companies (collectively "Punj Lloyd Group") are unable to exercise control or ensure or guarantee the integrity of/over the contents of the information contained in e-mail transmissions and further acknowledges that any view, opinion or advice expressed in this message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Punj Lloyd  Group.
Although we have taken all reasonable precautions to ensure that this communication is free from viruses. We do not assume responsibility for any loss or damage arising from the use of this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...